Improve Scuff & Mar Resistance of Water-based Ink

By Hywelt Technical Team · Published 2026-11-04 · Reading time ~5 min

After printing, the decorated surface must survive handling, packing, friction and heat pressing. Scuff and mar resistance depends on wax type, overprint varnish and ink film cure. This guide lists the levers engineers can pull.

Typical failure phenomena

Root-cause checklist (in priority order)

1. Wax type & level

2. Overprint varnish

3. Ink film cure

4. Stacking & cooling

Practical step-by-step solutions

  1. Blend PE wax and PTFE wax in the ink per supplier recommendation.
  2. Add a cross-linkable water-based overprint varnish on top.
  3. Raise oven temperature to ensure full film cure.
  4. Cool sheets 30 minutes before stacking.
  5. Run a Sutherland rub test and a nail-scratch test at QC.

Need technical support or sample?

Send your substrate specification, machine parameters and failure photos. Our application engineer in Hangzhou will reply with a targeted recommendation and lab sample.

Send technical inquiry Request sample

Frequently asked questions

Which wax is best for scuff resistance?

PTFE wax gives the lowest coefficient of friction; PE wax gives hardness. A blend works best.

Can I add more wax to solve scuff?

Up to a point. Beyond the recommended level, wax blooms to surface and ruins adhesion and gloss.

Does overprint varnish always help?

Yes, if it is chemically compatible with the ink underneath. Test a small batch first.