Moving from Solvent-based to Water-based Inks and Coatings
Most solvent-to-water projects fail on drying, not on chemistry. Water carries a different evaporation profile, so a press that runs comfortably on solvent ink can be drying-limited on water-based at the same speed and film build.
The second most common failure is colour: shades that match on a drawdown do not necessarily match at production opacity and speed. Both issues are predictable, and both are cheap to test before a line is committed.
Where this application fails
- Speed has to be cut on the water-based version because the existing dryer cannot remove the water at full output.
- Colour matched on a laboratory drawdown drifts at production speed and film thickness.
- Cleaning, waste and press-side handling change more than expected, and operators improvise.
How Hywelt approaches it
- Drying capacity is measured first, at your line speed and film build — this decides whether a switch is feasible on the existing dryer.
- Film treatment and substrate are confirmed next, since water-based adhesion is less forgiving of inconsistent corona than solvent systems.
- A staged trial runs one colour or one job through the full sequence — print, dry, convert — before the line is committed.
Products used in this application
| Product | Range |
|---|---|
| Water-based Gravure Surface Printing Ink | Waterborne & Printing Inks |
| Water-based Gravure Ink for Shrink Film | Waterborne & Printing Inks |
| Water-based Ink for PVC Decorative Film | Waterborne & Printing Inks |
What we need before quoting
| Current system | Solvent ink type, line speed, film build, dryer configuration |
|---|---|
| Substrate | Film or paper, treatment method and consistency |
| Constraints | Speed and quality that cannot be given up |
| Conversion | Downstream steps the print must survive |
Frequently Asked Questions
Sometimes, at reduced speed. Drying capacity is measured at your line speed and film build during the trial, and the result states what the existing dryer actually achieves — rather than assuming it is sufficient.
Drift depends on opacity and film thickness at production speed. Colour is matched at production conditions during the trial, with a stated tolerance, so the comparison is like for like.
A staged switch — one product family or one colour first — is the usual route. It limits exposure while the drying and handling questions are answered on real work.
Related pages
Contact Hywelt
Email: [email protected] (site inbox)
Overseas main: [email protected]
WhatsApp: +86 13216144789