Water-based Surface Printing Ink for Flexible Packaging
In surface printing the ink is the outer and only layer. There is no laminate to protect it, so the print carries the whole burden: scuffing in the bag maker, blocking on the wound roll, rub resistance in transit, and odour or solvent residue in the packed product.
Water-based surface inks address the solvent side of that problem, but only if drying capacity and film treatment are handled honestly — those two decide whether the switch works on your press.
Where this application fails
- Blocking and set-off on tightly wound rolls when residual solvent or moisture stays in the film stack.
- Adhesion loss on BOPP/OPP where the corona level drifts between deliveries.
- Odour or solvent residue complaints on food-adjacent packaging after the switch to water-based.
How Hywelt approaches it
- Film type and treatment level are confirmed first — adhesion is tested at the treatment you actually run, not at a laboratory optimum.
- Print speed, drying and rewind tension are tuned on trial, and block resistance is checked under wound-roll conditions rather than on single sheets.
- Where the print contacts food or faces migration limits, the end use is stated before any compliance screening; claims are released only after verification.
Products used in this application
| Product | Range |
|---|---|
| Water-based Gravure Surface Printing Ink | Waterborne & Printing Inks |
| Water-based Gravure Ink for Shrink Film | Waterborne & Printing Inks |
What we need before quoting
| Film | PE, OPP/BOPP, thickness, corona or surface treatment level |
|---|---|
| Press | Gravure, line speed, cylinder engraving, drying capacity per colour |
| Packing | Wound roll diameter and tension, bag-making or filling step |
| End use | Product contact or not, migration limits, odour sensitivity |
Frequently Asked Questions
Suitability depends on the specific grade and the migration limits of the end use. State the application in the inquiry; compliance screening is performed before any claim is made — we do not publish certifications we do not hold for a given grade.
Usually the drying curve is the limiting factor in a solvent-to-water switch. Send line speed and dryer configuration and we will state what the trial showed, rather than assume the existing dryer is sufficient.
Colour matching is done against a reference print with a stated tolerance. Some very high-opacity or metallic effects behave differently in water-based systems and are flagged before the trial, not after.
Related pages
Contact Hywelt
Email: [email protected] (site inbox)
Overseas main: [email protected]
WhatsApp: +86 13216144789
Send substrate, process and end-use details for a quotation — response within 1 business day. English / Spanish / Russian support.